Mechanical and physical properties of fiberboard bonded by palm-based polyurethane resin at different equivalent weight ratios and hot pressing temperatures / Mohd Norhisham Sattar
Medium density fibreboard is normally produced with urea-formaldehyde (UF) and/or phenol-fonnaldehyde adhesives. However, the former is considerably toxic and environmentally damaging where the formaldehyde emissions are found to cause negative health effects such as cancer. As an alternative, Malay...